1573 Carroll St, Brooklyn, NY 11213
1573 Carroll St, Brooklyn, NY 11213
Oct 14, 2026
Brick itself can last a century or more. The mortar holding it together usually doesn't. That's why most brick maintenance comes down to two jobs: keeping water out of the wall, and catching failing mortar before it turns into damaged brick.
The routine isn't complicated. But a few common habits do real harm, like blasting a wall with a pressure washer or sealing it with a coating that traps moisture. Here's what to do, what to skip, and which NYC rules apply.
Most of this takes an hour or two a year.
| Task | How often | What you're checking |
|---|---|---|
| Walk the exterior | Twice a year, spring and fall | Cracks, crumbling mortar, flaking brick, stains, plants in the joints |
| Clean gutters, check downspouts | Twice a year | Overflow staining, water discharging onto the wall |
| Look again after storms and hard freezes | As needed | New cracks, loose brick, water stains inside |
| Clear weep holes | Every few months, if your wall has them | Blockages from paint, caulk, or debris |
| Rinse salt off stoops and lower courses | Early spring | White deposits, eroded joints near the ground |
| Professional inspection | Every 5 to 10 years, sooner on older or exposed walls | Mortar depth, hidden moisture, lintels, parapets, chimneys |
| Repointing | Commonly every 25 to 30 years, depending on mortar, exposure, and workmanship | Joints eroded past 1/4 inch |
Weep holes are small drainage openings that appear on cavity walls and brick veneer. Many older solid brick walls don't have them.
You don't need tools beyond a screwdriver, a camera, and binoculars.
Water causes nearly every brick problem. It enters through open joints, cracks, and leaks, then freezes and expands by about 9 percent. Do that dozens of times a winter and mortar crumbles and brick faces pop off.
Most of the prevention is housekeeping:
If efflorescence keeps coming back after you clean it, the water source hasn't been fixed.
The National Park Service's guidance is to use the gentlest means that works. Preservation Brief 1 recommends starting at 100 psi or below, even a garden hose, and stepping up only as needed, generally no higher than 300 to 400 psi.
| Method | Verdict |
|---|---|
| Garden hose, soft bristle brush, non-ionic detergent | Best first choice |
| Low-pressure wash, 100 psi or below, rarely above 300 to 400 psi | Acceptable, after a test patch |
| Power washing | Avoid on a brick facade. It can erode the surface and push water into the wall |
| Sandblasting or grinding | Never. It strips the protective surface and can't be undone |
| Metal brushes | Avoid. NPS says to use bristle brushes only |
| Acid cleaners | Leave to a professional, with a test patch first |
Test a small, hidden area before you clean the whole wall. If the brick or mortar looks worse after the test, stop.
You'll see advice online to reseal brick every few years. For older NYC buildings, the guidance goes the other way.
The National Park Service says a masonry wall that's watertight and in good repair shouldn't need a water-repellent coating. Paint and film-forming sealers can trap moisture inside the wall, which leads to spalling that's often hidden until the coating fails. The Brick Industry Association also discourages colorless coatings on most exterior brick, and recommends siloxane products if one is ever used.
So fix the source of the water first. A breathable water repellent is a last resort, and it's something to discuss with a mason before anyone sprays it on.
Salt is the main threat. De-icing products can draw moisture into brick and mortar and contribute to scaling and erosion, especially near the ground.
Ivy and other climbing plants root into joints and hold moisture against the surface. Pull vines back and keep shrubs a few inches off the wall so air can move and you can see what's happening behind them.
Mortar is the part of a brick wall that wears out first, and it's meant to. Here's how to read what you find.
| Joint condition | What it means | What to do |
|---|---|---|
| Hard, intact | Sound | Clean only |
| Eroded past 1/4 inch | Water can get in | Plan repointing within a year or two |
| Crumbling, powdery, or open | Failing | Repoint soon, and check for water damage behind it |
How the job is done matters as much as when. The old mortar needs to come out to a depth of 2 to 2.5 times the joint width, with a minimum of about 3/4 inch. The new mortar has to be softer than the brick. Hard modern cement mortar on old soft brick traps moisture and can spall the brick faces. Our guide to common repointing mistakes covers where jobs go wrong, and our brick pointing service page covers what we handle.
Some buildings can't just wait for the next convenient summer.
| If your building is... | Rule | What it means |
|---|---|---|
| Taller than six stories | Facade Inspection Safety Program (Local Law 11) | A licensed engineer inspects the facade every five years. An Unsafe condition needs protection, like a sidewalk shed, immediately, and carries monthly penalties |
| Landmarked or in a historic district | Landmarks Preservation Commission approval | Approval is needed before repointing, even with matching materials. A wrong mortar color or composition is a common violation |
| Any building needing scaffold or a shed | Separate permits | Scaffolding has its own permit, whatever the landmark status |
The facade program exists because of a real death. In 1979, a Barnard College student was killed by falling masonry on Broadway, which led to Local Law 10 the following year. Under the current rules, per RAND's FISP fact sheet, an uncorrected Unsafe condition costs $1,000 a month plus a charge based on the length of the shed.
An uncured landmark violation can carry a fine of up to $5,000, plus up to $250 a day after that. Smaller buildings aren't under FISP, but an owner is still liable if masonry falls.
NYC pricing depends on height, access, and how much of the wall is open. These are typical contractor ranges.
| Scope | Typical NYC cost |
|---|---|
| Localized repointing or patching of a section | $5,000 to $15,000 |
| Full repointing of a three-story brownstone facade | $18,000 to $40,000 |
| Scaffolding, often a separate line | $10,000 to $25,000 |
Catching failing joints while only a few areas are open keeps you in the first row. Waiting until the whole facade is open puts you in the second, and if the brick itself has started to spall, brick replacement gets added on top.
Don't wait for the next scheduled walk-around if you see:
NY Vanta Contractors has been serving NYC for over 28 years, and handles brickwork in Brooklyn, the Bronx, Manhattan, and Queens. Brooklyn and Manhattan have many landmarked blocks, where the approval step comes before any work.
Check it twice a year, in spring and fall, and after severe weather. Plan a professional inspection every 5 to 10 years. Mortar commonly needs repointing every 25 to 30 years, though that varies with the mortar, the exposure, and the quality of the original work.
Usually not on an older building. The National Park Service says a watertight, well-maintained wall shouldn't need a water-repellent coating, and film-forming sealers and paint can trap moisture and cause spalling. Fix the water source first.
Avoid it. Start with a garden hose and a soft bristle brush. If more is needed, NPS guidance is to stay generally below 300 to 400 psi and test a small area first. Never sandblast.
Efflorescence, mineral salts left behind when moisture moves through the wall and evaporates. It isn't harmful on its own, but it points to a water problem. Brush it off dry, and find the source.
Press a screwdriver into a joint. If it sinks in more than 1/4 inch, or the mortar is crumbling, powdery, or missing, it's time to plan repointing.
A well-kept brick wall can last 100 years or more. The mortar is the maintenance item, not the brick.
If the building is landmarked or in a historic district, you need Landmarks Preservation Commission approval before the work starts. Otherwise repointing on its own usually doesn't need a separate DOB permit, but scaffolding or a sidewalk shed does need its own permit.
If you've found crumbling joints, flaking brick, or cracks you're not sure about, get a free estimate or call (718) 593-4048. We'll tell you what the wall needs, and what it doesn't.
Licensed NYC Concrete Contractor